WASTE GLASS CEMENT MORTAR MODIFIED WITH PALM FRUIT FIBRE
Abstract
The use of waste glass as fine aggregate in mortar is limited by Silica-Alkali Reaction (SAR), which can cause expansive silica gel formation, cracking, and structural instability—especially at high replacement levels. This study investigates palm fruit fibre (PFF) as a mitigation strategy for SAR in mortar containing 40% waste glass. PFF was added at 0%, 0.5%, 1.0%, 1.5%, and 2.0% by cement weight, and mortar mixes were tested for workability, compressive strength, flexural strength, density, and water absorption at curing ages of 3, 7, and 28 days. Results showed that PFF dosage significantly influenced performance. Compressive strength increased with curing age, with the 2.0% PFF mix nearly matching the control at 28 days. Flexural strength improved consistently with both curing age and fibre content, with 2.0% PFF achieving the highest tensile resistance. Regression models developed for compressive and flexural strength showed strong predictive accuracy (R² = 0.97 and 0.96), validating the influence of curing age and fibre dosage. The compressive model revealed a minimal negative effect of PFF, while the flexural model confirmed its positive contribution. Although higher PFF levels reduced workability, the fibre effectively mitigated SAR-induced strength loss and enhanced tensile performance. A fibre content of 1.5–2.0% is recommended for balancing strength, durability, and workability. The modified mortar is suitable for plastering, bricklaying, and non-load-bearing applications where sustainability and crack resistance are prioritized.
Keywords:
compressive strength, flexural strength, waste glass mortar, alkali-silica mitigation, palm fruit fibrePublished
How to Cite
Issue
Licensing
Copyright (c) 2026 ABDULRAHMAN GARBA, AHMAD SANI, IBRAHIM ALIYU ADAMU

This work is licensed under a Creative Commons Attribution-NonCommercial 4.0 International License.